Dear sir,
 
you can uer the following
 
1) ESAB OK 67.15 which is basic electrode of Esab
2) OK 67.13 of Esab
3) diffusaloy 910 of diffusion engineers
 
Regards

On Mon, Sep 7, 2009 at 11:51 AM, GOPU NAIR <gopunair5343@yahoo.com> wrote:
Dear all
 
I want to weld  longitudal and circumfential seams of A240Tp310 plate  to form a cylindrical shell (pressure part). Design Pressure is below 10Kg/cm2 and Design temp is below 200 deg.C. Could you suggest the most suitable consumable for SMAW which will not develop hot cracks during welding. Electrodes of Indian origin or locally available preferred.
 
Thanks in advance
 
Gopu


Love Cricket? Check out live scores, photos, video highlights and more. Click here

--
Amarjit Singh

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...