Hi Dear

Please refer to QW 202.3 of Sec IX it is clearly given for fillet weld repairs.

 

Regards

Harikumar Dayalan

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of prabhakar s
Sent: Thursday, September 10, 2009 6:32 PM
To: materials-welding@googlegroups.com
Subject: [MW:3154] Re: Repair Weld

 

Hi,

 

thank you very mch for your prompt reply. But our client is not accepting the repair work with GTAW process. How to convince them? Can you tell me how to convince them with the code backup document?

 

Your early response in this regard will be highly appreciated.

 

Regards

Prabhakar. S

On Wed, Sep 9, 2009 at 1:00 PM, sreedhar ch <sdchitturi@gmail.com> wrote:

When you have the WPS for each welding process either seperately or a combined one , you can do the repair on fillet weld.

 

Chitturi

On Wed, Sep 9, 2009 at 12:41 PM, prabhakar s <prabhakars84@gmail.com> wrote:

Hi,

 

We have to repair a fillet weld joint which is welded by SMAW process. Material is SS (A312 Gr316L). Can we do the repair with GTAW? Is it allowed as per any code? Please give me the reference also.

 

 

We have a WPS for GTAW process on SS Material (A312 Gr316L).  

 

Regards

Prabhakar. S

 

 

 

 



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...