[MW:3163] RE: 3162] RE: 3161] Re: 3156] Suppliers/manufacturers of seamless pipes

 As per my knowledge ISMT Limited  dont manufacture red API 5 L pipes . They  manufactures pressure tubes/pipes to various international specifications like BS 3059 Part I and Part II, BS 3601, BS 3602, DIN 17175 (St 35, St 45, 15 Mo3, 13 Cr Mo44, 10 Cr Mo910), ASTM A-53, ASTM A-106, ASTM A-179, ASTM A-192, ASTM A-209 (TI), ASTM A-210, ASTM A-213 (T11, T12, T22), and equivalent for high temperature / pressure service in boilers, high / low temperature and high pressure service in heat exchangers. Producing tubes in the range of 6 to 273 mm OD.

 

Find attached ISMT broacher with contact detail of ISMT. You may pls check with them.

 

Contact:

1)

The  Indian Seamless Metal Tubes  Ltd.   ismtbby@gnbom.global.net.in   T:-022-26542020/2021 F:-022-26542177 The Metropalitan Building,East Wing,2nd FloorBandra-Kurla Complex,Bandra(E),Mumbai-51


or

2) Mr. N. Kalyan
Executive Vice President - Marketing- ISMT Limited,Lunkad Towers, Viman Nagar,Pune - 411 014
Email:
kalyan@ismt.co.in



From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nachhattar Singh
Sent: 11 September 2009 14:02
To: materials-welding@googlegroups.com
Subject: [MW:3162] RE: 3161] Re: 3156] Suppliers/manufacturers of seamless pipes

You can check with ISMTL  - Indian Seamless Tubes Limited – Baramati

 

Regards 


 


 

 

Nachhattar Singh

Director

Phone: 91-22-2758 0044 - 91-98201 81158

Fax:91-22-27580033

Email:n.singh@moodyint.com

Web: www.moodyint.com

Web: www.edn.com.au

 

Moody International (I) Pvt Ltd

32 / 33 Gautam Complex , Sector - 11
C.B.D Belapur , Navi Mumbai - 400 614
Maharashtra (India)

Mumbai

Maharashtra

400 614

India

 

 

 

 

    

           

     

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shashank Vagal
Sent: Friday, September 11, 2009 1:47 PM
To: materials-welding@googlegroups.com
Subject: [MW:3161] Re: 3156] Suppliers/manufacturers of seamless pipes

 

Thanks, Rupesh. I have tried some of these, they do not manufacture seamless. Any way, let me do it all over again. Shashank Vagal

--- On Fri, 11/9/09, prashant pansare <prashantpan_99@yahoo.co.in> wrote:


From: prashant pansare <prashantpan_99@yahoo.co.in>
Subject: [MW:3159] Re: 3156] Suppliers/manufacturers of seamless pipes
To: materials-welding@googlegroups.com
Cc: Rupesh.Jambhale@mottmac-india.com
Date: Friday, 11 September, 2009, 10:19 AM

Rupesh,

Thanx for providing such type of information to all of our members.

Thanx again,

Rgards

PSP( IRS )

--- On Fri, 11/9/09, Jambhale, Rupesh A <Rupesh.Jambhale@mottmac-india.com> wrote:


From: Jambhale, Rupesh A <Rupesh.Jambhale@mottmac-india.com>
Subject: [MW:3158] RE: 3156] Suppliers/manufacturers of seamless pipes
To: materials-welding@googlegroups.com
Date: Friday, 11 September, 2009, 9:43 AM

Find below vendor list in India

 

Regards,
Rupesh A. Jambhale

Vendor Name

Country

Contact Person

Email ID 

Website

Telephone No

Fax no

Address (Head Office)

Address (Mumbai Office)

Work Address

JINDAL SAW LTD

MUMBAI

Mr. Mishra

info@jindalsaw.com

www.jindalsaw.com

HO:91 (11) 26188360-74 / Mum:91 (22) 23513000 / Works:91 (2551) 230712-716,
230239-240

HO:91 (11) 26170691 / Mum: 91 (22) 23521889 / Works:91 (2551) 230967

Jindal Centre,
12 Bhikaiji Cama Place
New Delhi 110066

Jindal Mansion,
1st Floor 5-A, G.
Deshmukh Marg (Peddar Road)
Near Jaslok Hospital
Mumbai - 400 026.

 

LALIT PIPES & PIPES LTD

MUMBAI

Mr. P.K.Mathew (Head Marketing)

HO-Mum:info@lalitsawpipes.com / Works:plant@lalitsawpipes.com

www.lalitsawpipes.com

HO-Mum:91 22 2756 1169 / Works:91 22 2756 1173

HO-Mum:91 2527 244161 / 65 / 66 / Works:91 2527 244061

212, Hermes Atrium,
Sector-11, C.B.D. Belapur,
Navi Mumbai-400 614, (India)

212, Hermes Atrium,
Sector-11, C.B.D. Belapur,
Navi Mumbai-400 614, (India)  

Survey No. 77,
Village Varaskol,
Khardi Rly. Stn. (C.R.)
Tal. Shahapur, Dist. Thane,
State : Maharashtra. (India)

MAHARASHTRA SEAMLESS LTD

MUMBAI

Mr. Gautama Atha

HO-Works:contact@mahaseam.com / Mum:mslkln@vsnl.net

www.jindal.com/msl.htm

HO-Works: 02194 38511 / Mum:91-22-24902570,72,74,76,78,80

HO-Works:02194 38513 / Mum: 91-22-24925473, 91-22-24901700

Pipe Nagar, Village Sukeli, Taluka Roha,
N.H.-17, B.K.G. Road,
Distt. Raigad-402 126 (Maharashtra)

402, Sarjan Plaza,
100, Dr. Annie Besant Road,
Opp Telco Showroom,
Worli, Mumbai - 400018

Pipe Nagar, Village Sukeli, Taluka Roha,
N.H.-17, B.K.G. Road,
Distt. Raigad-402 126 (Maharashtra)

MAN INDUSTRIES LTD

MUMBAI

Mr. Roy Chowdhary - GM (Marketing) / Mr. Mandar: 9930457912

uday.roy@maninds.org'; 'enquiry@maninds.org'

www.mangroup.com

Tel : +91-22-6647 7500 /
2610 8888,

Fax : +91-22-66477 600

Man House, 102, S.V. Road, Vile Parle (W),
Mumbai - 400 056 INDIA

Man House, Vile Parle (W)
Mumbai 400 056

Village : Khedoi,
Taluka : Anjar,
Dist.: Kutch (Gujarat), (INDIA).
Tel. : +91-2836-275751 / 275752
Fax : +91-2836-275750

SURINDRA ENGINEERING & CO. LTD (MUKUT PIPES LTD)

MUMBAI

Mrs. Dsouza / Mr. V M Harugade

HO-Mum:surindra@vsnl.com,
ajit@mukat.com 

www.mukat.com

HO-Mum:91-22-2851 5940 / 1 / 2 / 3 / 4

HO-Mum:91-22-2851 0129

Surindra House, M.V.Road Safaid Pool,P.O. Box No. 8939, Next to Sakinaka.Tel. Exchange, Andheri (E) Mumbai – 400 072. (India)

Surindra House, M.V.Road Safaid Pool,P.O. Box No. 8939, Next to Sakinaka.Tel. Exchange, Andheri (E) Mumbai – 400 072. (India)

 

PSL INDIA LTD

MUMBAI

 

krishna@pslltd.co.in ; 'dnsehgal@pslltd.co.in'; 

 

 

 

PSL Towers, Marol, Andheri(E), Mumbai 400 059

PSL Towers, Marol, Andheri(E), Mumbai 400 059

 

RATNAMANI METALS & TUBES LTD

CHHATRAL, GUJRAT

 

HO:info@ratnamanitech.com / Mum:info.mumbai@ratnamani.com / Works:info.sstp@ratnamani.com

www.ratnamani.com

HO:91-79-2741 5501/2/3/4 / Mum:91-22-2380 2591/2/3/4 / Works:91-2764-232254 / 232263 

HO: 91-79-2748 0999/ Mum: 91-22-23876464/ Works:91-2764-234105

17, Rajmugat Society,
Naranpura Cross Roads,
Ahmedabad - 380 013
Gujarat (India). 

44, C.P.Tank Road,
Mumbai - 400 004.
Maharashtra (India).

Survey No. 769,
Ahmedabad –Mehsana Highway,
P.O. Chhatral –382 729,
Ta: Kadi, Dist: Mehsana.

WELSPUN GUJRAT STAHL ROHREN LTD

MUMBAI

 

Mr. B. K. Mishra
 / Jiji  Cherian 

HO-Mumbai:sales_wgsrl@welspun.com / Works:sales@wgsrl.com

www.welspunpipes.com

HO-Mum:91 22 66136000 / Works:91 2641 256011 / 256281

HO-Mum:91 22 2490 8020/ 2490 8021 / Works:91 2641 256285

Welspun Gujarat Stahl Rohren Limited (W.G.S.R.L.)
Trade World, B-wing, 9th Floor,
Kamala Mills Compound,
Senapati Bapat Marg, Lower Parel,
Mumbai - 400 013 India.

Trade World, B-wing, 9th Floor,
Kamala Mills Compound,
Senapati Bapat Marg, Lower Parel,
Mumbai - 400 013 India. 

Village Vadadla, Near Dahej,
Taluka:Vagra (6 kms before Dahej),
Bharuch -Dahej Road, District Bharuch,
Gujarat 392 130 India.

MAHAVIR SEAMLESS TUBE PVT LTD ( STOCKIT & DISTRIBUTOR )

MUMBAI

RAHUL.M.VORA/M.H. VORA 

mahavir@vsnl.com ; rahul_vora@yahoo.com

www.mahavirtube.com

23427580/23420291/23449729/23414638 

22-23434083 

240, NAGDEVI STREET,MUMBAI-3 

240, NAGDEVI STREET,MUMBAI-3 

nil

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shashank Vagal
Sent: 11 September 2009 09:22
To: materials-welding@googlegroups.com
Subject: [MW:3156] Suppliers/manufacturers of seamless pipes

Dear sir,

We have received an inquiry for supply of the following seamless pipes:

API 5L, Dia 12-14", Grade X60-65. (Thicknesses not provided at this stage)

Overall lengths, 32 km Prodn Line (Sour service severity 1); 23 km Water Inj Line (Sweet Service); 21 km Gas Export Line (Sour service severity 3).

Is the sour service severity grading as given adequate and correct?

2500 Joints, 4" Sch 40 pipes, (Spec not provided at this stage, but most likely to be API 5L GrB)
Please let me know if you know any parties who can supply these items to us.

Best regards,

Shashank C Vagal


 Moody Group Confidentiality Note:  The information transmitted is intended only for the person(s) or entity to which it is addressed.  It may contain confidential and/or privileged information or material.  Any review, retransmission, dissemination to other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and delete the material from any computer.

 

______________________________________________________________________


This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

 


Beauty is just a click away. Find beauty parlor listings on Yahoo! India Local

 


See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz.

 

  

 

 
 

email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step