Wednesday, September 9, 2009

[MW:3152] RE: 3150] Repair Weld

Dear friend

Yes, you can use GTAW WPS for Fillet Repairs only.

Where as for Groove repair welding, your WPS as to be qualified for QW – 451.2

In case of Fillet repair weld, as per QW – 451.4 your WPS is applicable to weld All fillet size.

 

Regards

Harikumar Dayalan

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of prabhakar s
Sent: Wednesday, September 09, 2009 11:41 AM
To: materials-welding@googlegroups.com
Subject: [MW:3150] Repair Weld

 

Hi,

 

We have to repair a fillet weld joint which is welded by SMAW process. Material is SS (A312 Gr316L). Can we do the repair with GTAW? Is it allowed as per any code? Please give me the reference also.

 

 

We have a WPS for GTAW process on SS Material (A312 Gr316L).  

 

Regards

Prabhakar. S



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35748] Re: PQR- Chemical testing requirements