Monday, September 7, 2009

[MW:3128] Welding of A240Tp310

Dear all
 
I want to weld  longitudal and circumfential seams of A240Tp310 plate  to form a cylindrical shell (pressure part). Design Pressure is below 10Kg/cm2 and Design temp is below 200 deg.C. Could you suggest the most suitable consumable for SMAW which will not develop hot cracks during welding. Electrodes of Indian origin or locally available preferred.
 
Thanks in advance
 
Gopu


Love Cricket? Check out live scores, photos, video highlights and more. Click here
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...