[MW:3124] zero gap weld on SS

Hello All

 

We prepare a project on piping in a air separation plant.

For liquid gases (LOX,LIN,LAR) we use 304L pipe and ER308L filler material.

 

For on small pipe (1-3") with 2mm wall on root pass please advice if we can weld with zero gap and no filler material.

Iulian OPREA

 



--~--~---------~--~----~------------~-------~--~----~