Hi

You can use ER80SB2 or ER 70S 2 and for SMAW use E8018B2  or E7018-1 However you have to qualify PQR . No need of SS electrode

Regards

 

Hegde

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Manoharan Kalimuthu
Sent: Friday, September 04, 2009 2:22 PM
To: materials-welding@googlegroups.com
Subject: [MW:3117] CS (A106 GR B) TO AS (A 335 P11)

 

Dear All,

                      Here in our project we have A106 GR B to A335 P11 Dissimilare welding ,Can any on suggest the filler wire and Electrode?

Is it possible to use ER309 and E309.

Regards

Mano

 



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...