[MW:2201] RE: 2187] RE: 2184] Ovality tolerance

For this Inner dimension (4300mm), if we  target %0,25. Is that mean about +-102mm ?

Regards,

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PB HEGDE
Sent: Wednesday, May 13, 2009 2:10 PM
To: materials-welding@googlegroups.com
Subject: [MW:2187] RE: 2184] Ovality tolerance

 

Dear Anil

 

Please refer UG80 of Sec VIII Div 1 You can have 1% ovality is acceptable but It is case to case basis i.e Higher the Dia , it should be kept less than 0.5% even the acceptable tolerance is high b) higher ovality will cause more offset in weld seam

ii) In case of heat exchanger , You can not afford to accept higher ovality . You should target less than 0.25% ,Higher ovality will give problem in tube bundle insertion.

Regards

 

Hegde P.B.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of N Anilkumar
Sent: Wednesday, May 13, 2009 4:04 PM
To: materials-welding@googlegroups.com
Subject: [MW:2184] Ovality tolerance

 

Dear All,

 

Can anybody tell me,

what's the ovality tolerance of cylindrical shell pressure vessel (ID 4300 mm and plate thickness 12mm).

 

Regards,

Anil

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 




__________ Information from ESET NOD32 Antivirus, version of virus signature database 4070 (20090513) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com


__________ Information from ESET NOD32 Antivirus, version of virus signature database 4081 (20090517) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Anonymous said…
Keep posting stuff like this i really like it

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...