Skip to main content

[MW:2263] Re: UT in lieu of RT

Thank for your promptly respone and highly appreciated. Unfortunately i don't have B31 code case (181 and 2235). Any one can share with me?
 

On Thu, May 28, 2009 at 11:21 AM, BR <raghurambathula@gmail.com> wrote:

assuming your design code is ASME B31.3 (else pl specify?) you can
refer old postings on the group, we have lot of dicussion in the past
on this subject.
refer code case 181
"ASME B31 committee has developed B31 Case 181 to permit the use of
UT, particularly TOFD in lieu of RT for B31.3 applications. ASME B31
case 181 was apparently taken from ASME Code Case 2235, which
addresses the UT examination in lieu of RT for vessels and not piping.

The major difference from what I can see between B31 case 181 and ASME
Code Case 2235 is the minimum wall thickness requirements and maybe
the acceptance criteria.

As we all know ASME B&PV codes looks at flaws by aspect ratios. a/l or
vertical height divided by length. That gives you the aspect ratio
which is then used to determine the maximum flaw size permitted. You
can actually accept cracks per the ASME B&PV code as long as they are
within the acceptable limits, but not with ASME B31.3.

After looking at the acceptance criteria for B31 Case 181, I see that
they are using the same philosophy.

Where ASME B31.3, Table 341.3.2 does not allow any cracks for RT and
in most cases no IF. Why would cracks be permitted with UT and not RT?
I believe the B31 Case 181 was taken from ASME Code Case 2235 and the
reference to cracks was inadvertently missed. When using TOFD you can
differentiate between linear indications and cracks. Does anyone know
of any reference by ASME B31 committee regarding this issue?"
Source: ndt.net



On May 28, 6:37 am, tong tong <tong...@gmail.com> wrote:
> Dear All members,
> I really need you expertise opinion on the above mentioned subject.
> Basically our project(new piping installation) requirement is RT but we
> having a lot of problems to do it. One of the major problem is the window
> which is very limited. To avoid any backlog i purpose to my boss to go for
> UT instead of RT. It is permissible by the code and standards to do UT
> instead of RT. Which code and standard we should refer?. Thank in advance
> for your kind cooperation



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...