[MW:2193] Re: 2140] SMAW consumable for the welding

Hi,

Kindly enligthen of what is meant by Eutectic Electrode.


Regs,

R.Ravi



On 5/11/09, PB HEGDE <hegde.pb@isgec.com> wrote:

Hi!

Welding of this type of material (Used in machine tool ) is very critical and require to be welded by Eutectic type electrode. With proper preheating and technique. (Generally it is of Ni base) . You can approach L& T eutectic  or MAGNA (Austrelian  Co) they have the range of electrodes or Tig wire

Regards

 

Hegde p.B.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sandy kumar
Sent: Monday, May 11, 2009 2:35 PM
To: materials-welding@googlegroups.com
Subject: [MW:2140] SMAW consumable for the welding

 

Hi friends

Can anyone please tell me which SMAW consumable I can use to weld following material combination :-

 

1st material:-

C.

Si.

Mn.

S.

P.

0.50%

0.25%

0.70%

0.05%

0.05%

2nd material :-C=0.355,Si=0.6645,Mn=1.7084,P=.0209,S=0.0326,Cr=0.2083,Ni=0.0333, Mo=0.0314,

Cu=0.0226,Al=0.0182,Ti=0.0177,V=0.0935,Nb=0.0103

Please suggest which I can use if it is not suitable.

Best regards

Sandeep Kumar

 




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...