As per API 650 clause 5.2.3.1 it is very much clear that plates to be joined by butt welding shall be matched accurately and retained in position during welding operation.

Also nowhere it is indicated about buttering or any other means to adjust such dimensional deviation which is beyond qualified WPS.

Only alternative is to replace shell plate /add one more such shell plate which will not violate Tee joint distance as per code.

Bharat B. Gole

 






Date: Sat, 28 Feb 2009 10:56:43 +0400
Subject: [MW:1663] Buttering on Plate
From: pkhormis@gmail.com
To: materials-welding@googlegroups.com

Dear All!!!
 
We are doing some Tanks as per API 650. In one of that tank ,we faced a problem like shortened the lingth of plate..and JOINT GAP became more than the required 'Root gap'. Almost   "55mm" we got .So we thought about 'Buttering'. But in API 650 not mentioned any thing about 'buttering'. So which standard we have to follow for it, and what are the test we have to conduct over there.
 
There was no PWHT as per WPS,Pre heat was only upto 40 ^0 C.
 
plate thickness is 23.4mm- 'Double 'v' groove' , ASTM 573.GR 70.

--
PRADEEP KUMAR HORMIS







Rediscover the magic of Windows & WIN a Windows Vista laptop & Windows mobile phone at www.windowsandme.com Try it now!
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...