Yes, Impact test is mandatory requirement as per material specification of SA 333 Gr -  1,3,4, 6,7,9 & 10, even it is not designed for low temperature services.

Regards,

Sridhar Doddapaneni

On Thu, Feb 26, 2009 at 5:36 PM, Faigal Fernando Agbanawag <faigal.agbanawag@czfp.com> wrote:

Dear all,

 

Can anybody elaborate chapter III of B31.3 regarding the impact test requirement of ASTM A333 where in section 323.2.2 states the limitation concerning impact testing  of a particular material. Is it mandatory for A333 to have an impact test ?,  where low temperature service is not an issue.

 

Your response are highly appreciated.

 

Regards,

 

Faigal Fernando Agbanawag
Sr. Piping Engineer
Clough ZFP

T +966 3 8828818 Ext: 241
F +966 3 8828622
M +966 (0) 507780576


Disclaimer: This email and any files transmitted with it are confidential and intended solely for the use of the addressee(s) named herein. If you are not the intended recipient or addressee, you should not use, disseminate, distribute, copy or alter this email. Any views or opinions presented in this email are solely those of the author and might not represent those of "CZFP".

Warning: Although reasonable precautions have been taken to ensure no viruses are present in this email, "CZFP" cannot accept responsibility for any loss or damage arising from the use of this email or attachments. If you have received this electronic mail message in error, please contact the sender directly.





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...