Dear All,
 
With ref to QW 200.4 (b) combination of process
PQR A - 15mm with SMAW process
PQR B- 40mm with SAW process
 
Wht is the base metal thk. qualified if we cobines WPS SMAW + SAW
Will it be 5 to 30mm(with both SMAW & SAW - 30mm or 5 to 200mm( with SMAW-30mm & SAW 200mm)
 
If any interprtation to this condition is there then it will very helpful
 


Thanks & Regards
Muhammed Ibrahim PK

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...