Wednesday, February 25, 2009

[MW:1632] Minimum strength requirement of procedure.

Hi friends,
 
I need clarification on one important thing regarding PQR.
 
PQR is qualified with SA516Gr.60 ( P1 Gr.1) to SA516Gr.70( P1 Gr.2) wth E7018-1 Electrode and it passes at 62 KSI strength
Can it be used for SA516Gr.70 to SA516Gr.70 production weld based on the above results?.
 
As the production material require 70 KSI strength, how this procedure will support for SA516Gr.70 to SA516Gr.70welding
 

Thanks & Regards
Muhammed Ibrahim PK

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...