Groove design is essential variable only for procedure qualification. For welders groove design is not an essential variable( please see Table 4.12 & Table 4.1) in AWS D1.1.
 
Regards,
 
Muhammed Ibrahim

2009/2/25 Radhakrishnan Venkatraman <r_venkat68@hotmail.com>

 

From: r_venkat68@hotmail.com
To: materials-welding@googlegroups.com
Subject: Essential variable as per AWS D 1.1
Date: Tue, 24 Feb 2009 16:54:42 +0000

My dept was having one PQR qualified as per AWS D1.1 with double V Groove weld.
When we try to qulify our welders for a specific project,where in the requirement is for single v groove weld.
We have Conducted the test with 16mm plate (Single V preparation)
The third party qualified the welders.Is this ok
 
Because as per AWS D 1.1 groove configuration is an essential variable
 
Is any one clarify this
 
Regards
R.Venkataraman  


Need more space to upload pictures? Get 25 GB online storage with Windows Live SkyDrive! Try it!

Akshay Kumar takes on the two reigning Bollywood Khans. Catch the action on MSN Entertainment! Check it out! --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...