Saturday, February 14, 2009

[MW:1585] Re: T,K,Y joints testing by UT

TKY Joints are to be checked by experienced UT operators who are to be additonally qualified using mock up test peice of TKY Configuaration and same mock up TKY test peices may be obtained from TWI or use TKY Qualified CPN operators rather than ASNT LEVEL II  UT operators .
Best Regards,
Francis Lobo

----- Original Message -----
From: Ali Asghari
To: materials-welding@googlegroups.com
Sent: Sat, 14 Feb 2009 13:53:18 +0530 (IST)
Subject: [MW:1580] T,K,Y joints testing by UT


Dear all

due to the geometry of the K,Y joint & limitation of access ,some area is missed during testing by ut in root and cap(especially in toe welds),now how can i aware about this area?
thanks adv



--
My life has changed. What about yours?
Log on to the new Indiatimes Mail and Live out of the Inbox! http://mail.indiatimes.com
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...