Friday, February 13, 2009

[MW:1572] Re: weld profile

Ali Asghari
 
Purpose of burr grinding - to enhance fatigue life of highly stressed weldments-ex- T-FP,T-Y-K Joints.
 
If you have access to AWS D1.1-2008 refer Section 8-Page 285.
Hope it helps




With Warmest Regards

Ganesan
H/P - 65 9189 6531 



 

 








 





Date: Thu, 12 Feb 2009 03:17:08 -0800
From: asghariali@rocketmail.com
Subject: [MW:1570] weld profile
To: materials-welding@googlegroups.com



----- Forwarded Message ----
From: Ali Asghari <asghariali@rocketmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, February 12, 2009 11:05:21 AM
Subject:



hi
i'm confused about following case that written in spec of my project:

When specified on the Project Drawings the weld toes shall satisfied API RP2A

sect.11 requirements. If necessary, the weld toe can be grinded to obtain the

required profile. In that case a rotary burr grinder (no disc grinder) shall be used,

as shown figure 5.1. Grinding shall produce a smooth concave profile at the weld

toe with the depth of depression penetrating into the plate surface to at least

0 . 5 m below the bottom of any undercut, but not deeper than 2mm or 5% of the

thickness, whatever the bigger, below the surface.(pl see the attachment)
0ne question:performing according to the figure,does it cause notch & stress concentration?
two question:is it detrimental for properties of joint?
three:the bigger or lesser,which one correct?
what is the philosophy of this statment?
which T,K,Y joint must be performed according above?
thanks adv
 
 



More than mail–Windows Live™ goes way beyond your inbox. More than messages
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...