Dear sri. Kabeer,
You can check with IOL wherein Argon is graded as I,II etc. IOLAR Grade 2 is used for pressure vessel application. A certificate to this effect with chemistry basically moisture content would be given IOLAR on demand.
Regards
Mohan Ananthanarayanan
DGM Qulaity ISRO
On Wed, 9 Oct 2013 11:54:42 +0800 (SGT), smkabeer ahamed wrote
>
>
> On Tuesday, 8 October 2013 11:51 AM, smkabeer ahamed <sm_kabeerahamed@yahoo.co.in> wrote:
>
>
> Dear friends,
>
> stainless steel welding ss304 to ss304 I have used TIG welding at groove
> joint.I have used argon gas purity level 99.7 percent instead of
> 99.99percent .our client suspect weld joint get oxidized.Is this purity
> level is accepted as per any code How we will check what percent of
> oxidation available in joint.is any testing method is there.how we will
> convince our client and get approval from him.kindly suggest as early as
> possible
>
> Regards,
>
> S.M.KABEER AHAMED
> CHIEF ENGINEER
> QUEST INSPECTION AGENCY
> BANGALORE-INDIA
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment