[MW:18952] Cryogenic plant (Nitrogen generating unit liquid & gas ) Process piping welding with normal ER 308l fillerwire

Dear Sir,

What's problem happen in future?

(1) If wr are using   ER 308L filler wire without carring lateral expansion at -196 in ss 304l process piping in cryogenic (Nitrogen generating) plant  (Liquid/gas  fluid).

(2) If we are using both filler wire ER 308L with lateral expansion (0.38mm ) at -196 degree. & ER 308L without lateral expansion. how to segregate the joints in this case.

regards 

lalit

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...