Yes require
Pandithan
On 11/15/12, Sanjay Yadav <ssy070707@gmail.com> wrote:
> PWHT is not required in your case as base metal thickness is only 20mm.
>
> On Sun, Oct 28, 2012 at 3:43 PM, Rems Okonkwo
> <rems.okonkwo@gmail.com>wrote:
>
>> Trichy,
>>
>> PWHT will not be required, the reference thickness consider during the
>> design calculation of the vessel is 20mm, the RF pad is only an
>> attachement.
>>
>> regards,
>>
>> Rems
>>
>> On Thu, Oct 25, 2012 at 3:56 PM, g.venkatesan06@gmail.com <
>> g.venkatesan06@gmail.com> wrote:
>>
>>> Dear experts,
>>> we are doing welding in a vessel of joint nozzle to dish with
>>> reinforcement pad(pipe thick 10mm(32inch), dish thik 20mm & RF pad 20mm)
>>> the weld detail in drawing shows bevel(55 degree) followed with
>>> fillet(10mm). All are P1 material.
>>> In my question : the total weld metal deposit is 50mm in a joint(40mm
>>> CJP
>>> & 10 Fillet)
>>> code says above 38mm groove weld for P1 material PWHT is mandatory and
>>> also says groove & fillet exceed 26mm in 2inch pipe PWHT is required.
>>> Now we will do PWHT or not in a particular joint. If not kindly tell the
>>> reason.
>>> Regards
>>> venkat
>>> welding engineer
>>> trichy.
>>>
>>> ----------
>>> Sent from my Nokia phone
>>>
>>> --
>>> To post to this group, send email to materials-welding@googlegroups.com
>>> To unsubscribe from this group, send email to
>>> materials-welding+unsubscribe@googlegroups.com
>>> For more options, visit this group's bolg at
>>> http://materials-welding.blogspot.com/
>>>
>>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>>
>>> The views expressed/exchnaged in this group are members personel views
>>> and meant for educational purposes only, Users must take their own
>>> decisions w.r.t. applicable code/standard/contract documents.
>>>
>>>
>>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>>
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment