Hi
 
Phosphorus is an Impurity and if it exceeds 0.05% reduces the ductility of steel and it can cause "Cold Shortness" i.e. cracking during cold working.
 
Regards
 
Prem Nautiyal
 
Cell: 9769316004
 

--- On Fri, 11/2/12, Pramod Kulkarni <prakul52@gmail.com> wrote:

From: Pramod Kulkarni <prakul52@gmail.com>
Subject: [MW:15834] Role of phosporous on weldability of steel
To: materials-welding@googlegroups.com
Date: Friday, November 2, 2012, 10:09 AM

 
Request to confirm why  Phosprous is very low in weldable steel ( 0.05 Maximum ).
How it affect weldability
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...