Thursday, November 1, 2012

[MW:15825] PWHT -9%Cr-1%Mo/V materials

Dear All,
 
I strongly desire to know why do we have to execute post weld heat treatment in 9%Cr-1%Mo/V alloys in more than one cicle to simulate repair when we are qualifying welding procedure specification?
 
Why not only do just one cicle after all the permissible repairs have been done?
 
Best Regards,

Guttemberg

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...