Re: [MW:14851] RE: 14845] Re:non purge wires for SS welding

Please note that Taseto - a 100% subsidary of Kobe Japan, also manufactures these and nomenclature is TGF - series.
There is one difference, in that unlike Kobe TGX- these are flux covered. The usage is the same successfully accepted in the welding industry.In case details are needed, please let me know.
 


 
On Thu, Jul 12, 2012 at 9:28 AM, Mohamed Elsayed ( BTG) <MElsayed@ccc.ae> wrote:

It is TGX wire used for from only Kobelco Manufature in Japan, SEE attached file for help.

It is too costly. You can SEE ( one rod from TGX= 1 Kg –in Price-of E7018-1,3.2MM..see!!!)

Thanks

Mohamed

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vijmukesh@gmail.com
Sent: 12 July 2012 06:37
To: materials-welding@googlegroups.com
Subject: [MW:14845] Re:non purge wires for SS welding

 

Dear all,

I would like to know about the non purge wires for SS welding. Please share your experience for these wires. Are these economical wrt normal GTAW wires with Ar purging.

Thanks
Mukesh Kumar

Sent from BlackBerry® on Airtel


From: "Ankit Patel" <ankit.patel@orientalindia.net>

Date: Sat, 7 Jul 2012 16:50:22 +0530

Subject: [MW:14790] Filler Materail required for welding SS 321 to SA 516 gr-70

 

Dear Experts,

 

I want to weld SA 516 GR-70 plate to SA 182 TP 321.

 

Kindly suggest me the filler material grade used  for welding this material.

 

Thanks & Regards

Ankit Patel
Engineer Quality

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...