Tuesday, July 10, 2012

Re: [MW:14831] USE of PQR for more than one Subcontractors

No, Each company should have their own procedure.

Thanks & Regards
Muhammed Ibrahim PK



On 10 July 2012 11:18, Parveen Kumar Nakwal <pknakwal@gmail.com> wrote:
Dear Experts.
 
Let us suposse client is A & B is Contractor.
Under B ( C,D & E are more 3 subcontractor companies are working).
 
WPS/PQR had been established by Subcontractor C only under the shadow of B.
SO can other subcontractors i.e D & E companies can use the same PQR.
 
please mention the clause no. as per ASME sec. IX, is it QW302 ?
 
Waiting for reply.
 
Parveen K. Nakwal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...