Re: [MW:14758] corrosion under pipe Supports

Dear Krish Barwar:
 
What kind of support are you talking about?
Is it welded to pipe?
What is the pipe and support material specification?
what about the diameter?
Is it a process or transportation piping?
 
I hope you can give us more information...
 
Best regards
 
Sent: Tuesday, July 03, 2012 7:52 AM
Subject: [MW:14754] corrosion under pipe Supports
 


Dear All,


please advice me for inspection  of corrosion under pipe Supports, But Without lifting the pipe from the support. I need to find a quick way of Inspecting the pipes at Each pipe support with some kind of handheld device and NDT to Identify, screen for severity and to measure the Defects Preferably Between the pipe and pipe support.

I tried with guided waves, with bad results. Has anyone successfully tested a system?


thanks


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...