Dear Asad,
Please clarify the charpy specimen size used during testing and the
testing impact temp
Reagrds
Vikas waghmare
On 7/2/12, rahul m <rahulmenator@gmail.com> wrote:
> * SA 387 GR 12 CL2, 65 THK. MDMT is -18 DEG CELCIUS how to make PQR for
> this thickness ? or how many PQR required for this thickness?*
>
> On Wed, Mar 14, 2012 at 2:31 PM, asad azmi <azmiasadayub@gmail.com> wrote:
>
>> Dear All,
>>
>> Greetings.
>>
>> A vessel is being fabricated as per ASME SEC VIII DIV 1.
>>
>> Vessel material is SA 387 GR 12 CL2, 65 THK. MDMT is -18 DEG CELCIUS.
>>
>> Approved WPS is supported by 2 PQR detailed as below --
>>
>> *PQR 1*
>> **
>> Test coupon thickness - 40 mm ,
>> Welding process used - GTAW + SMAW + SAW ,
>> Weld deposit by SMAW Process is 19 mm.
>> Weld deposited by SMAW is impact tested at 0 deg celcius.
>> **
>> *PQR 2*
>>
>> Test coupon thickness - 10 mm ,
>> Welding process used - GTAW + SMAW ,
>> Weld deposit by SMAW Process is 8 mm.
>> Weld deposited by SMAW is impact tested at - 18 deg celcius.
>> **
>> *Whether PQR 2 can be used for SMAW Process to deposit 21 mm weld in
>> a weld groove of 65 mm in depth .( for closing seam of shell to dished
>> head
>> & nozzle to dished head weld seam)*
>> **
>> Please advice. please give ASME SEC IX Reference.
>>
>> Thanks & Regards
>>
>> Asad Azmi
>> **
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-