Dear experts. I am facing a problem in boiler water wall TUBES SA 213 T12 grade material. The main problem is when we try to weld tube to tube spiral weld wide root gap comes 6 to 8 mm. Can we weld the joint with same root gap. As I know root gap is not essential variable for WPS. Can we go further with this wide root GAP ? If distortion comes during welding then what is the acceptance criteria as per various ASME, AWS. Section in RT? We try to come these two tubes closer with hydraulic jack after welding we found CRACK due to over stress. Can spool Piece is only solution of this type of joint? Please suggest me. VISHWAS. (QA/QC)
Sent from BlackBerry® on Airtel
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...