6% Moly Stainless Steels, Duplex and Alloy 20 may serve your purpose.
Krishna
On Jul 5, 7:51 pm, "Nachhattar Singh" <nsi...@librainspection.com>
wrote:
> Dear Experts
>
> I have an issue where the media to be deployed is FeCL3 solution so under
> these
>
> conditions what should be the MOC. The item to be made is valve to be fitted
>
> on the tank and the connecting piping.
>
> Please suggest
>
> Nachhattar Singh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment