Materials selection, welding, forming, Heat treatment, corrossion, NDT
Dear All,
Please suggest me any information about PCM (Parameter Crack Measurement).
Regards,
Firman
ExxonMobil recommend a cracking parameter value of 0.23 for NACE defined sour service. The formula used is as follows:Pcm = C + Si/30 + (Mn+Cu+Cr)/20 + Ni/60 + Mo/15 + 5B
Post a Comment
Dear sir , Can you share references/Documents @ james Gerald ? On Mon, Apr 29, 2024 at 9:11 PM 'james gerald' via Materials & ...
1 comment:
ExxonMobil recommend a cracking parameter value of 0.23 for NACE defined sour service. The formula used is as follows:
Pcm = C + Si/30 + (Mn+Cu+Cr)/20 + Ni/60 + Mo/15 + 5B
Post a Comment