[MW:9228] Hardness Issue


Dears:
 
Could you please tell me what can I do to solve this issue?:
 
1.- HV hardness requirement for X-60 1" wt pipeline girth welds: 248 HV
2.- Of 15 measurements one value reached 285 HV .
3.- The weld is under water righ now.
 
How can we solve this?, I think just to support, because we can't take the pipe out.
 
Regards.


Eduardo Calva



  > --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...