Pipes
The purpose with a pipe is the transport of a fluid like water, oil or similar, and the most import property is the capacity or the inside diameter.
For a ASME/ANSI B 36.10 Welded and Seamless Wrought Steel Pipe the inside diameter - ID - of a NPS 2 inches pipe with
- schedule 40 is 2.067"
- schedule 80 is 1.939"
The inside diameters are close to 2" and the nominal diameter related to the inside diameter. Outside diameter are 2.375" for both schedules.
Since the outside diameter of a single nominal pipe size is kept constant the inside diameter of a pipe will depend on the "schedule" or the thickness of the pipe. The schedule and the actual thickness of a pipe varies with the size of the pipe.
It is common to identify pipes in inches by using NPS or "Nominal Pipe Size". The metric equivalent is called DN or "diametre nominel". The metric designations conform to International Standards Organization (ISO) usage and apply to all plumbing, natural gas, heating oil, and miscellaneous piping used in buildings. The use of NPS does not conform to American Standard pipe designations where the term NPS means "National Pipe Thread Straight".
Nominal Bore (NB) may be specified under British standards classifications along with schedule (wall thickness).
The tolerances are looser to pipes compared with tubes and they are often less expensive to produce.
Tubes
The nominal dimensions of tubes are based on the outside diameter. If we look at Copper Tubes - ASTM B88 the outside diameter of a 2" pipe is 2.125", relatively close to 2".
The inside diameter of a tube will depend on the thickness of the tube. The thickness is often specified as a gauge. If we look at Copper Tubes - ASTM B88 the wall thickness of 0.083"of a 2" pipe is gauge 14.
Any one can explain what the real difference between pipe and tube.
--
Pravez Alam
Doha Qatar
Mob#+9746813248
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments