RE: [MW:7725] P No-A No

As per ASME Section IX 2010th edition S numbers are deleted , all are merged as P number

Bharat B. Gole




Date: Sat, 23 Oct 2010 07:09:11 +0530
From: k7moorthi@yahoo.co.in
Subject: Re: [MW:7722] P No-A No
To: materials-welding@googlegroups.com

 

1. P number - Parent material Group
2. S number - Sub group of  Parent material
3. F number - Filler material group
4. Group Number - Group
5. A number - Chemical Analysis Group


 
175, R.Kesavamoorthi,
Principal surveyor,
Quest (pvt.) Ltd.,
Ranipet.



From: Noushad cp <ncp.clt@gmail.com>
To: materials-welding@googlegroups.com
Sent: Fri, 22 October, 2010 4:33:29 PM
Subject: [MW:7716] P No-A No

Dear all,
 
 
Can anyone define the following?
 
 
1.P number
2. S number
3. F number
4.  Group Number
5. A number
 
 
Noushad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...