Saturday, October 16, 2010

Re: [MW:7591] forming head

Sorry, I don't answer your question but please tell the thickness and
which portion crack happened, such as on weld, on knuckle or other.

Thanks

On Sat, Oct 16, 2010 at 7:09 PM, Navid Navidi <navid_751400@yahoo.com> wrote:
> Hello All,
> We are going to form a head for a presser vessel. Its diameter is about 3000mm.
> And it is made of A516Grade70. Unfortunately, while forming we have cracks on
> the material which cause rejection of the head.
> How can we form a crack-free head? Do we have to do the forming in several
> steps? Do we need heat treatment between forming steps?
> Thank you,
> Saied
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
Regards,

T. Rizal Hidayat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...