Dear Hemant,
100% radiography means all but weld joints have to be radiographed irrespective of thickness of plate or Pipe size .Hence, Exemptions mentioned in UW-11 for Full RT is not possible in case of 100% RT.
Full radiography means you can take advantage of exemptions mentioned in UW-11.
ASME code specifies only Full,Spot and No radiography but not 100% RT .
Generally, Owner's specification calls for 100% RT .
Hope this will help.
Regards,
Manish
"hemant solanki" <h_solanki@rediffmail.com> Sent by: materials-welding@googlegroups.com 13/10/10 10:56
|
|
Dear All,
Could you please tell me what is the difference between 100% radiography & fully radiography? Is it clarified in ASME code?
Thanks,
Hemant Solanki
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment