Re: [MW:7325] Can we do painting prior to hydrotest?

Dear Friends ,
Query was regarding piping system of 4 km in Pipe rack  not for pressure vessels . In India also painitng  prior to pressure testing is genrally not a practice  for shop fabrication specially  in case of pressure vessels. 

 ----- Original Message -----
From: GOSWAMI Pradip -THERMAL
To: materials-welding@googlegroups.com
Sent: Fri, 1 Oct 2010 22:43:53 +0530 (IST)
Subject: [MW:7313] Can we do painting prior to hydrotest?

Satish,   ASTM has a standard, E-1003, for hydrotest, which clearly specifies that "New systems should be tested prior to painting, where practical".   The responses posted by Mr Arunachalam cites several discussions and replies on the same issue. I've also attached the gist of the article by J.E.Batey, which was published in, ASNT journal materials evaluation.   If you look at ASME Sec-VIII,DIV-1,UG-99,(see below):-   (k) Vessels, except for those in lethal service, may be painted or otherwise coated either internally or externally, and may be lined internally, prior to the pressure test. However, the user is cautioned that such painting /coating /lining may mask leaks that would otherwise have been detected during the pressure test. The above sentence  implies "do it at your risk and be ready for the consequences". ASME as a code have to be fabricator friendly, but for Lethal Services failures due to suggested  wrong practices would mean liability. However at the same time fabricator have to exercise  judgement and good engineering practice.   Depending on the type of paints used, paints will have tendency to mask defects or hinder meaningful inspection. If the vessel or piping is subject to PWHT, any defect noted during hydrotest, would call for repair and re-stress relieve, the time and money spent on rework may out-weigh your initial gain.   Generally in North American utilities (Nuclear) painting before hydro test is not an accepted practice. The same guidelines are followed by large oil Companies also. An extract from such a specification :-   ·         Hydrostatic pressure testing shall be performed prior to the application of paint or other protective coatings to the welds and heat affected zones, unless otherwise approved by the Principal.   I would say, given a choice painting shall always be done after hydro test. If the project is a rush and time is a constraint, painting of piping or vessel may be done, leaving welds and at least 2 " on each side as unpainted during hydrotest, which would be painted following hydrotest.   Thanks.   Pradip Goswami,P.Eng. Welding & Metallurgical Engineer/Specialist Email-pgoswami@sympatico.ca, pgoswami@quickclic.net      
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Satish Hingalkar
Sent: Friday, October 01, 2010 2:10 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:7300] Can we do painting prior to hydrotest?
 
Dear all members,
Thanks for reply on my query.
As suggested by you guys, i can say to contractor to go ahead for painting before hydrotest by holding more time up to all visual check of joints. I have one more concern as: As per company specification, we are doing 10%MT & 10%RT that is OK or we have increase the % of MT & RT.
Please respond.
Regards,
Satish  
On Thu, Sep 30, 2010 at 2:05 PM, <francis.lobo@indiatimes.com> wrote:  
Dear All,
In the modern fast track projects these deviations are common , You can accept the deviation provided you extend the hold time for min 4 hrs for joints not seen or painted with chart recorder and accounting any pressure variation with tempt,

This is practiced in most of the offshore projects. However for onshore /subsea pipeline hold period is 24hrs and pressure variations vs. tempt accounted.
Francis Lobo

----- Original Message -----
From: Bathula Raghuram (Mumbai - PIPING)
To: 'materials-welding@googlegroups.com'
Sent: Thu, 30 Sep 2010 15:03:40 +0530 (IST)
Subject: RE: [MW:7285] Can we do painting prior to hydrotest?
Interesting, and you have a valid point but nothing is proven, until then just go with the flow (tried and tested methods). No Inspector would be happy but bound to accept as per code.  remember your company specification prohibits it and you are intended to accept, hence code reference is given, Masking of any discontinuity by thin layer of paint, may be yes perhaps may be not. If you refer the paragraphs of these codes which will give a cautionary statement at the end "painting/coating may mask the leak". Normally weld joints are left open and rest of the area is painted before hydro. In my opinion 105 bar is too high for a layer of paint to with stand, or you may allow only blasting and priming before hydro and final coating after hydro. If I remember correctly only Australian code AS1210 prohibits it.  
From: Satish Hingalkar [mailto:shingalkar@gmail.com]
Sent: Thursday, September 30, 2010 12:49 PM
To: Bathula Raghuram (Mumbai - PIPING)
Subject: Re: [MW:7283] Can we do painting prior to hydrotest?
 
Hi,
Thanks for prompt reply
Piping system of having pipe rack near about 4 KM,service-Nitrogen,Code ASME B31.3
As u said,ASME B 31.3 allows, but my query is that whether painting will affect the joint leak detection normally found in hydro test??
As per my knowledge, Painting has ability to penetrate and plug/ seal off small pin holes which are normally detected in hydro test.      After curing, paint can withstand pressure in small pin holes that can obstruct the leaks. But during operation, paint can be decomposed and start leaking, please comment.
Regards,
Satish
On Thu, Sep 30, 2010 at 7:27 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
You have not specified the type of component, fluid and design code. ASME code for both vessels and piping have this provision. Sec VIII div 1 allows except for lethal service (UG 99) and B31.3 allows except for sensitive leak testing (345.3.1)
 From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Satish Hingalkar
Sent: Wednesday, September 29, 2010 11:55 PM
To: Materials & Welding
Subject: [MW:7276] Can we do painting prior to hydrotest?
 Dear Members,
 Our contractor has raised a design change request for painting prior to hydrotest.As per COMPANY specification, painting to be carried out after successful completion of hydrotest,but contractor wants to do painting before hydrotest,can we accept this deviation? if  we want to accept the deviation, what criteria to be follow??
 Our design conditions are 105 barg hydrotest pressure and design temp.85 deg.c,NDT is 10% MT & 10% RT.
 Waiting for reply. Pl.respond ASAP.
Regards,
Satish
 
 





--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.




--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...