Tuesday, October 26, 2010

[MW:7816] Re: is there any method by which we can strat RT BY REMOTE CONTROL SYSTEM ?

Dear Aslam khan,

You can do RT with X ray machine which have the system of safe
elapsing time.You canadjust the paramerers and switch on the
machine .The exposure will on after a pre set time of few minutes and
during that time the RT technician can be at a safe distance.


Thanks and regards,

MUHAMMAD TUFAIL

On Oct 25, 5:02 pm, aslam khan <aslamkha...@gmail.com> wrote:
> hi friends ,
> we strat RT to move crankshaft manually .is there any method by which
> we start RT BY REMOTE CONTROL SYSTEM FOR SAFTETY OF RT
> TECHNICIANS?THANKS
>
> REGARDS
> M.ASLAM KHAN
> QA/QC ENGINEER
> DESCON ENGINEERING LTD.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...