Dear All,
Design Code – ASME B31.3
Welding Code – ASME BPV SECTION IX
I have a PQR for the following material classification as per ASME BPV SEC IX
Material – P1 Group No. 1 to P1 Group No. 2
Weld Metal Impact Tested – Yes
My query is that,
1. Is there any problem for welding P1 Group No.1 to P1 Group No.1 & P1 Group No.2 to P1 Group No.2 based on above PQR?
2. Can I write separate WPS (with impact test) based on above PQR for,
Material – P1 Group No. 1 to P1 Group No. 1
Material – P2 Group No. 2 to P2 Group No. 2
My next query is that,
Is there any problem for showing all material range in a single WPS based on above PQR?
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment