[MW:3129] Re: Welding of A240Tp310


ESAB OK 67.15 can be used for this material and should be available in India. ESAB OK 67.13 can also be used. OK 67.15 is a fully basic electrode wich should be safer in regards to hot cracking.

Regards


Claes Gillenius
Development Engineer, MMA. (Spec. stainless and non Fe-alloys)
Direct tel:  +46 (0)31 509315
Mobile +46 (0)707532012
Company                ESAB AB
Address                  Box 8004, 402 77  Gothenburg, Sweden
                                 LindholmsallĂ©n 9
Company  reg number        556005-7738



GOPU NAIR <gopunair5343@yahoo.com>
Sent by: materials-welding@googlegroups.com

2009-09-07 08:29

Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
[MW:3128] Welding of A240Tp310





Dear all
 
I want to weld  longitudal and circumfential seams of A240Tp310 plate  to form a cylindrical shell (pressure part). Design Pressure is below 10Kg/cm2 and Design temp is below 200 deg.C. Could you suggest the most suitable consumable for SMAW which will not develop hot cracks during welding. Electrodes of Indian origin or locally available preferred.
 
Thanks in advance
 
Gopu



Love Cricket? Check out live scores, photos, video highlights and more. Click here


This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...