--- On Sat, 5/9/09, PB HEGDE <hegde.pb@isgec.com> wrote:

From: PB HEGDE <hegde.pb@isgec.com>
Subject: [MW:3119] RE: 3117] CS (A106 GR B) TO AS (A 335 P11)
To: materials-welding@googlegroups.com
Date: Saturday, 5 September, 2009, 2:09 PM

Hi

You can use ER80SB2 or ER 70S 2 and for SMAW use E8018B2  or E7018-1 However you have to qualify PQR . No need of SS electrode

Regards

 

Hegde

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Manoharan Kalimuthu
Sent: Friday, September 04, 2009 2:22 PM
To: materials-welding@googlegroups.com
Subject: [MW:3117] CS (A106 GR B) TO AS (A 335 P11)

 

Dear All,

                      Here in our project we have A106 GR B to A335 P11 Dissimilare welding ,Can any on suggest the filler wire and Electrode?

Is it possible to use ER309 and E309.

Regards

Mano

 






See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...