Wednesday, February 25, 2009
[MW:1626] FW: Essential variable as per AWS D 1.1
From: r_venkat68@hotmail.com
To: materials-welding@googlegroups.com
Subject: Essential variable as per AWS D 1.1
Date: Tue, 24 Feb 2009 16:54:42 +0000
My dept was having one PQR qualified as per AWS D1.1 with double V Groove weld.
When we try to qulify our welders for a specific project,where in the requirement is for single v groove weld.
We have Conducted the test with 16mm plate (Single V preparation)
The third party qualified the welders.Is this ok
Because as per AWS D 1.1 groove configuration is an essential variable
Is any one clarify this
Regards
R.Venkataraman
Need more space to upload pictures? Get 25 GB online storage with Windows Live SkyDrive! Try it!
Akshay Kumar takes on the two reigning Bollywood Khans. Catch the action on MSN Entertainment! Check it out!
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Subscribe to:
Post Comments (Atom)
Blog Archive
-
▼
2009
(2497)
-
▼
February
(184)
- [MW:1489] Re: Cladding Pipe Manufacturer
- [MW:1488] Re: 1474] Re: Required API 650 personal ...
- [MW:1491] Re: Cladding Pipe Manufacturer
- [MW:1492] Re: Cladding Pipe Manufacturer
- [MW:1499] Re: Dent in pipe
- [MW:1493] Re: HYDRO TEST OF VESSELS
- [MW:1494] Re: Dent in pipe
- [MW:1495] Re: Required API 650 personal for Bahrai...
- [MW:1496] RE: 1488] Re: 1474] Re: Required API 650...
- [MW:1497] Re: 1482] ASME VIII
- [MW:1498] RE: 1497] Re: 1482] ASME VIII
- [MW:1501] Re: Dent in pipe
- [MW:1500] Resistance welding testing lab-Reg
- [MW:1502] percentage of RT
- [MW:1503] Request to members
- [MW:1504] RE: 1500] Resistance welding testing lab...
- [MW:1505] Re: Resistance welding testing lab-Reg
- [MW:1506] National Welding Seminar 2009- Feb 4th-6...
- [MW:1508] Re: Resistance welding testing lab-Reg
- [MW:1507] Re: Resistance welding testing lab-Reg
- [MW:1509] NDT after hydrotest for ASME Sec VIII Di...
- [MW:1511] cheron crack detected by ut
- [MW:1510] Re: NDT after hydrotest for ASME Sec VII...
- [MW:1518] Significance of HOT PASS
- [MW:1512] Re: cheron crack detected by ut
- [MW:1513] RE: 1511] cheron crack detected by ut
- [MW:1514] Re: 1511] cheron crack detected by ut
- [MW:1515] Re: cheron crack detected by ut
- [MW:1516] painting
- [MW:1517] RE: 1516] painting
- [MW:1519] Re: 1516] painting
- [MW:1528] RE: 1518] Significance of HOT PASS
- [MW:1520] RE: 1517] RE: 1516] painting
- [MW:1521] Re: Significance of HOT PASS
- [MW:1522] Re: Significance of HOT PASS
- [MW:1527] RE: 1517] RE: 1516] painting
- [MW:1526] RE: 1518] Significance of HOT PASS
- [MW:1525] Re: painting
- [MW:1524] Re: painting
- [MW:1523] Re: Significance of HOT PASS
- [MW:1529] Re: 1516] painting
- [MW:1530] Re: painting
- [MW:1533] RE: 1518] Significance of HOT PASS
- [MW:1532] Re: Significance of HOT PASS
- [MW:1531] RE: 1518] Significance of HOT PASS
- [MW:1541] Re: Significance of HOT PASS
- [MW:1534] minimum length
- [MW:1535] Re: minimum length
- [MW:1536] RE: 1535] Re: minimum length
- [MW:1537] Re: minimum length
- [MW:1538] Min Separation of welds
- [MW:1539] RE: 1538] Min Separation of welds
- [MW:1540] Re: 1535] Re: minimum length
- [MW:1544] Re: Resistance welding testing lab-Reg
- [MW:1542] Re: Min Separation of welds
- [MW:1543] Re: Min Separation of welds
- [MW:1545] RE: 1542] Re: Min Separation of welds
- [MW:1546] torque value
- [MW:1547] Re: torque value
- [MW:1548] Re: Min Separation of welds
- [MW:1549] Re: torque value
- [MW:1550] burn thrugh
- [MW:1551] MIG Brazing of SF Cu pipes
- [MW:1552] Re: Min Separation of welds
- [MW:1553] Re: burn thrugh
- [MW:1554] RE: 1553] Re: burn through
- [MW:1555] Re: 1553] Re: burn through
- [MW:1557] Burn through
- [MW:1556] RE: 1555] Re: 1553] Re: burn through
- [MW:1558] WPS,PQR for tig welding for ss304 at 4.5...
- [MW:1559] RE: 1555] Re: 1553] Re: burn through
- [MW:1560] Re: NDT after hydrotest for ASME Sec VII...
- [MW:1561] NAB Nickel Aluminum Bronze
- [MW:1562] RE: 1560] Re: NDT after hydrotest for AS...
- [MW:1564] API 1104> Qualification of Repair Proced...
- [MW:1563] API > 1104 Welder Qualification Thicknes...
- [MW:1566] Re: API 1104> Qualification of Repair Pr...
- [MW:1565] A good suggestion from a member
- [MW:1570] weld profile
- [MW:1569] Re: 1555] Re: 1553] Re: burn through
- [MW:1567] RE: 1565] A good suggestion from a membe...
- [MW:1568] Re: torque value
- [MW:1571] Some clarifications for BS EN 15614-1 : ...
- [MW:1574] Re: weld profile
- [MW:1573] RE: 1571] Some clarifications for BS EN ...
- [MW:1572] Re: weld profile
- [MW:1575] FW: IIM course on Corrosion
- [MW:1576] RE: 1573] RE: 1571] Some clarifications ...
- [MW:1577] Re: 1565] A good suggestion from a membe...
- [MW:1579] Re: torque value
- [MW:1578] Re: weld profile
- [MW:1580] T,K,Y joints testing by UT
- [MW:1586] RE: 1579] Re: torque value
- [MW:1583] flash butt welding
- [MW:1585] Re: T,K,Y joints testing by UT
- [MW:1584] Re: weld profile
- [MW:1582] Nominal Thickness
- [MW:1581] Mix up of A106 Gr.B and A336 Gr.6 pipes
- [MW:1592] Re: Mix up of A106 Gr.B and A336 Gr.6 pi...
- [MW:1591] Re: Nominal Thickness
- [MW:1590] Re: Mix up of A106 Gr.B and A336 Gr.6 pi...
- [MW:1589] Re: Mix up of A106 Gr.B and A336 Gr.6 pi...
- [MW:1588] Re: Mix up of A106 Gr.B and A336 Gr.6 pi...
- [MW:1587] Re: weld profile
- [MW:1593] FILLER WIRE FOR TIG WELDING AT 4.5K ( - ...
- [MW:1594] Welding consumables (2.25Cr-1Mo-0.25V) w...
- [MW:1595] RE: 1593] FILLER WIRE FOR TIG WELDING AT...
- [MW:1596] Fw: Mix up of A106 Gr.B and A336 Gr.6 pi...
- [MW:1597] Re: 1593] FILLER WIRE FOR TIG WELDING AT...
- [MW:1598] Pneumatic test of Reinforcement Pad for ...
- [MW:1601] Re: Pneumatic test of Reinforcement Pad ...
- [MW:1599] Re: Pneumatic test of Reinforcement Pad ...
- [MW:1600] RE: 1599] Re: Pneumatic test of Reinforc...
- [MW:1602] RE: 1598] Pneumatic test of Reinforcemen...
- [MW:1603] Re: 1599] Re: Pneumatic test of Reinforc...
- [MW:1604] Dissimilar Welding combination of T12#T2...
- [MW:1605] Re: 1599] Re: Pneumatic test of Reinforc...
- [MW:1606] Welding presentation
- [MW:1607] Re: Dissimilar Welding combination of T1...
- [MW:1608] Technical Query (Welding of P No.9B with...
- [MW:1610] API 5L X85
- [MW:1609] Api 650
- [MW:1612] Re: 1599] Re: Pneumatic test of Reinforc...
- [MW:1611] Re: API 5L X85
- [MW:1616] Re: Technical Query (Welding of P No.9B ...
- [MW:1615] Re: API 5L X85
- [MW:1614] Re: API 5L X85
- [MW:1613] Re: API 5L X85
- [MW:1617] WPS from 2 PQRs
- [MW:1618] Re: WPS from 2 PQRs
- [MW:1619] FW: API 5L Gr B and A 106 Gr B
- [MW:1620] PIPE SA106GRB
- [MW:1621] RE: 1620] PIPE SA106GRB
- [MW:1622] RE: 1620] PIPE SA106GRB
- [MW:1638] Re: WPS from 2 PQRs
- [MW:1623] RE: 1622] RE: 1620] PIPE SA106GRB
- [MW:1624] RE: 1623] RE: 1622] RE: 1620] PIPE SA106...
- [MW:1625] Re: 1623] RE: 1622] RE: 1620] PIPE SA106...
- [MW:1626] FW: Essential variable as per AWS D 1.1
- [MW:1627] PLEASE SEND REPLY
- [MW:1628] Before You Ask
- [MW:1629] Re: PLEASE SEND REPLY
- [MW:1630] Standards for calibration of welding mac...
- [MW:1631] Re: FW: Essential variable as per AWS D ...
- [MW:1632] Minimum strength requirement of procedur...
- [MW:1633] Minimum impact energy value of PQR
- [MW:1634] Re: Minimum strength requirement of proc...
- [MW:1637] Re: Minimum impact energy value of PQR
- [MW:1636] Re: Minimum strength requirement of proc...
- [MW:1635] Combination of PQRs
- [MW:1640] Re: FW: API 5L Gr B and A 106 Gr B
- [MW:1639] flatolet
- [MW:1642] Re: FW: API 5L Gr B and A 106 Gr B
- [MW:1643] Re: flatolet
- [MW:1641] Re: flatolet
- [MW:1644] RE: 1638] Re: WPS from 2 PQRs
- [MW:1645] Re: Combination of PQRs
- [MW:1647] Re: 1638] Re: WPS from 2 PQRs
- [MW:1646] FAILURE DURING PNEUMATIC TESTING
- [MW:1648] Re: 1638] Re: WPS from 2 PQRs
- [MW:1649] comparison highlights for ASME sec VII...
- [MW:1650] RE: 1642] Re: FW: API 5L Gr B and A 10...
- [MW:1651] WPS parameter
- [MW:1652] Re: 1638] Re: WPS from 2 PQRs
- [MW:1653] Re: WPS parameter
- [MW:1655] A333 Material for impact test requiremen...
- [MW:1654] Difference between Full & 100 % radiogra...
- [MW:1656] Re: A333 Material for impact test requir...
- [MW:1657] Re: A333 Material for impact test requir...
- [MW:1658] Re: Difference between Full & 100 % radi...
- [MW:1659] Re: A333 Material for impact test requir...
- [MW:1661] Re: FW: Essential variable as per AWS D ...
- [MW:1660] Re: Nominal Thickness
- [MW:1662] Re :[MW:1660] Re: Nominal Thickness
- [MW:1664] voltage
- [MW:1663] Buttering on Plate
- [MW:1666] Re: Buttering on Plate
- [MW:1665] Highlights for ASME sec VIII, Div2 (U2...
- [MW:1686] knuckle joint
- [MW:1667] Re: Buttering on Plate
- [MW:1668] Re: Highlights for ASME sec VIII, Div2...
- [MW:1669] Re: Buttering on Plate
- [MW:1670] Re: Buttering on Plate
- [MW:1671] Re: voltage
-
▼
February
(184)
No comments:
Post a Comment