Consider higher end pressure 

On Sat, 2 Jul 2022 at 19:50, Manikandan J <mechmani22@gmail.com> wrote:
Dear All,

We have conducted a hydro test of Piping Spools (14'' Pipe x 12 Mtr Long),we have  faced Gauge pressure difference at Higher and lower end.

Test Pressure Required : 283 PSIG

Lower End  : 290 PSIG
Higher End : 283 PSIG

Kindly provide what is acceptable pressure difference between lower and higher end.

Regards,
Pradeepan.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmOG_p74j5MnzJ0ELbmDWCa7gnB0e2%2B13KP1B7TTv3EKdA%40mail.gmail.com.
--
Regards
Ramesh Babu Balaram
Head QA/QC
Zetwerk Manufacturing Businesses Private Limited
Mobile: +91 98 4 053 13 55

>>>DONATE NOW<<<
SUPPORT ZETWERK'S CAMPAIGN TO FEED THE VURNERABLE MIGRANT FACTORY WORKER POPULATION.
Contribute generously. Each donation will go towards essential ration kits.
Let's come together as a nation so that they don't have to go hungry

This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2nx%3DKqzye5zBrKWpOb%3DhNbyPCsadu3rbYdbX1X1pNM9gg%40mail.gmail.com.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...