Sunday, July 3, 2022

Re: [MW:33197] NI200 TO SS304 WELDING FILLER WIRE

Dear Sujith kumar, 
please refer API RP 582 for consuables selection
and below consubales are refered by API  
1.  ERNiCrFe-2 or -3. &   ENiCrFe-2 or -3.
2.  ERNi-1 & ENi-1.
check with consumable manufacturer they may suggest some other newly developed consumables based on this application  

However, it is highly recommended to use Nickle base consumable (Ni-1) as it is suitable consumable for NI200 alloy welding and better to avoid SS consumable for this joint as it may create crack on Ni alloy side due to dilution in the weld.


Regards,

Srinivas Rao


On Saturday, July 2, 2022 at 6:20:28 PM UTC+4 gerry_tup@yahoo.com wrote:
USE ERNI-1   (GTAW)       & ENi-1    ( SMAW)

Thanks & Regards

J.Gerald Jayakumar




On Saturday, 2 July, 2022 at 04:42:56 pm GMT+4, sujit kumar <sujitku...@gmail.com> wrote:


Hello experts.

Hope all is well.

I want to do welding of NI200 to SS 304  which filler wire I should use for that.



Best regards.
S.K

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/69834b4e-cf81-4c1a-86b9-49b0d2d9d393n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/563c8c3a-78c5-4507-97b5-49a41443da39n%40googlegroups.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...