Saturday, July 2, 2022

Re: [MW:33194] NI200 TO SS304 WELDING FILLER WIRE

USE ERNI-1   (GTAW)       & ENi-1    ( SMAW)

Thanks & Regards

J.Gerald Jayakumar




On Saturday, 2 July, 2022 at 04:42:56 pm GMT+4, sujit kumar <sujitkumar19942@gmail.com> wrote:


Hello experts.

Hope all is well.

I want to do welding of NI200 to SS 304  which filler wire I should use for that.



Best regards.
S.K

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/69834b4e-cf81-4c1a-86b9-49b0d2d9d393n%40googlegroups.com.

No comments:

[MW:35544] WELDING OF SS 310 MATERIAL CRACK ISUUE..

We are doing a welding of SS 310 Material Plate with ER310 Grade welding electrode... But its contineous cracking.... at welding line,,,,......