Skip to main content

Re: [MW:30663] TPI approval on WPS

For projects in middle east it is almost mandatory that a TPI is used although it is not a code requirement. In other countries u may follow what is prevailing in those countries.

Thanks & Rgds.
Prakash Gotimukul
Authorised Inspection Supervisor
AIA LLC TX USA
MOB +97155 7114671
           +919730039755

On Thu, Mar 26, 2020, 13:56 Vinay Thattey <vinay.thattey@gmail.com> wrote:
Nice explanation , Mr Ramesh

On Tue, 24 Mar 2020 at 08:37, Ramesh <rameshkannandevaraj@gmail.com> wrote:
Each organisation can certify WPS/PQR. refer ASME Sec-IX- QW 201,  TPI review/witness is NOT mandatory,

TPI review / witness is Not code requirements, this is to satisfy customers that they have qualified WPS/PQR  upfront with third party check than vendors own personal. 

Also note, code allows SWPS - Prequalified WPS, means u can understand that does not require TPI involvement ! 


Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Mon, Mar 23, 2020 at 3:06 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
No. TPI can witness PQR and can review WPS. TPI can't Certify PQR and can't Approve WPS. In ISO as examining body, they can certify WPQR not WPS. 

On Sun, 22 Mar 2020 12:38 pm Venkat Ramana, <venkatgps.ramana@gmail.com> wrote:
The contracted prepared and qualified as per AWSD1. 1 edition 2015 and ASME Sec IX edition 2015. Is there any requirement to do the sign on WPS copies??

Please clarify.... 

Venkat

On Sat, Mar 21, 2020, 12:29 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Not necessarily. But as per 2019, competent welding personal should be available to review welding related documents within company. 

On Sat, 21 Mar 2020 9:34 am Venkat Ramana, <venkatgps.ramana@gmail.com> wrote:
Dear Experts,

My query is that, is there any mandatory by TPI approval (Seal and Sign) on every WPS ?? even though they have already sign into the supporting PQR'S....

KINDLY CLARIFY WITH RELEVANT CODES AND STANDARDS.


Thanks & Regards

Venkat
+91 9676061257

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsPJvRAQu5%3DeNN0L8qFX_-SjVMCK-YAkoQ2AjshHsBmPdw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePi1hUtNnLbEdw6tT-vPZq8wPbTgQCbvYR8xfP7fbr2eQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsOHNyJEOu7CKyA62d7_vGtwonZ6g-9tUkMzGyLsOajiRQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMhbPUbSBZj156rMD%3D6y4Qpq6a1h%2BOpCiOiJLMvxn-ApA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcFcxi4PfXwvhAgPZCZHiCHCARw%2BSXoH%3DAijFi38x28o7w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OgfihoFZkoTKtiotyfTMf3qv%2BSmEn%3D%2BUPGdUUY_E%2BcjVw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4q%2Bx%2B1DKrCTeFR5hRzqPDupLNrx61QmoW7-bD%3DXP_cBStw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...