Re: [MW:30628] Interpretation of standard as Per ASTM A6 /A6M for Material MTC tensile Testing Requirement

I agree with your interpretation, one Test  for minimum Thickness and one Test for maximum Thickness provided both belongs to same Heat.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, March 12, 2020, 01:42:49 PM GMT+7, Mayur Hiremath <hiremath.qaqc@gmail.com> wrote:


Good Morning,
Dear Specialist,

It has raised me a doubt based on the Client comments, hence requesting for the clarification form Specialist of the below points as stated in the ASTM A6/A6M.

image.png

1)      According to the table B & Table C from ASTM A6/ A6M (Refer attached Snap Shot of the Page).  With Reference to the attached MTC Grade A572 Gr50, Client has Comment Required 2 Tensile test according to ASTM A6/A6M. Hence Commented and Rejected the MTC. Please kindly explain about the Validity of the Comment.

Scenario 1 My Interpretation of standard as per ASTM A6/ A6M

2)     According to the Table B:  As per my understanding is, when the Manufacturer Mill if rolling two separate Thickness (Example: 12MM plate and 50 mm Plate) form the Same Heat Number irrelevant to batch number / Plate Number. Then we need to have 1 tensile test for each one. (Example: 12MM plate one sample tensile test will be taken and need to be reported in the MTC of that Result and Other 50MM plate one sample tensile test will be taken and need to be reported in MTC, hence here total only 2  No tensile is conducted for each one thickness).

         As per my understanding is, when the Manufacturer Mill if rolling only 12mm Thickness (Example: 12MM plate) form the one Heat Number irrelevant to batch number / Plate Number. Then we need to have 1 tensile test for that one. (Example: 12MM plate one sample tensile test and need to be reported in MTC, hence here total only 1 No tensile is conducted for that one thickness).

 Scenario 1 Client Interpretation of standard as per ASTM A6/ A6M 

3)     According to the Table B:  As per Client understanding is, when the Manufacturer Mill if rolling two separate Thickness (Example: 12MM plate and 50 mm Plate) form the Same Heat Number irrelevant to batch number / Plate Number. Then we need to have 2 Separate tensile tests for each one. (Example: 12MM plate 2 tensile test and need to be reported in the MTC and Other 50MM plate 2 tensile and need to be reported in MTC, hence here 4 Nos of tensile is conducted for each 2 for one thickness).

           As per client  understanding is, when the Manufacturer Mill if rolling only 12mm Thickness (Example: 12MM plate) form the one Heat Number irrelevant to batch number / Plate Number. Then we need to have 2 tensile test for that one heat Number. (Example: 12MM plate 2 sample tensile test and need to be reported in MTC, hence here total only 2 No tensile is conducted for that one thickness). 

Total 3 page Nos Attachments Snap shot of the pages.

1)     ASTM A6 / A6M

2)     MTC Copy of the Minmetals Yingkou medium plate Co, Ltd (Heat No / Batch No: 12Thk 19105410A/1955874, 12Thk 19205764A /1960419, 12Thk 19205561A/195588, 25Thk 19205529D/201905260214) Certificate No: D070015082019B073036 Date of Issue 2019-07-09, Grade A572 Gr.50

3)     Snap shot of client Comment highlighted in Red Cloud Mark.

 

 Once again thanks in Advance and waiting for your Explanations.

Regards,
A.B.Hiremath.
QA/QC Department

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGQ515zGhUwy9TzjssNCCYdyyV3jV7A_jAgQPQQjN_YHsAJ7MA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...