Re: [MW:30592] Filler Wire Selection For SA240 TYP 304/404L Plate For pressure Vessel Welding requirement Ferrite No.- 3-5 FN

it will be very difficult to achieve your required ferrite in this material and std filler. Ask manufacturer for your requirement. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Mar 4, 2020 at 2:44 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
1. Check with the Welding consumable  manufacturer whether they produce ER308L with your Ferrite requirement.
2. Check for ER308 consumable, as your service condition being low temperature application, by proper welding condition sensitization could be avoided and higher carbon produces a more austenitic structure.

If the above 2 conditions do not work then you can try other alternative.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, March 4, 2020, 03:30:24 PM GMT+7, Atul Jha <atulkrjha21@gmail.com> wrote:


Dear Experts

 To obtain  Ferrite No. 3-5 FN After Welding of SA 240 TYP 304/304L Plate material which filler wire shall be used keeping below requirement under consideration :-

Mechanical Requirement :- As per ASME Boiler & Pressure Vessel Code.

Additional mechanical requirement Impact @ -196 degree celsius :-  minimum Lateral Expansion 0.38 mm. 

Welding Process : GTAW/SAW.

Service Type :- Cryogenic Service ( LNG Fuel Tank).

Approximate Job Dimension ;- THK 12 mm DIA. 5 meter Length - 30 meter.

Home Work Done :- I wish to do PQR With ER 310  Wire  ( Cost Approx INR  550 Rs/Kg ).
                  OR With ER 320 ( BUT here I have doubt that may Be ferrite obtained after welding Varies from 0-3 FN. Cost is also a constraint Approx INR 3000 Rs/Kg).

Kindly Guide if any other filler wire is available  & work done in past to obtain fulfill above requirement.

Regards
Atul Jha.


 


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/016fae51-1e6c-4f8f-bb21-10d1da01f4b6%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1836875463.2876829.1583313135648%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOkgRYMuoR9aJR2FBjX8008huEpuJU-ZP8bH%3D8vMyw3ZA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...