Refer para 7.4 of SAES-W-01*
Thanks
Muneeb.
On Mon, Feb 4, 2019, 7:15 PM Revdiwala Darshan <darshanmrevdiwala@gmail.com> wrote:
It depends on your production joint material.If X65 and above then PQR shall be qualified with same material.Regards,Darshan--On Mon, 4 Feb 2019, 1:26 pm puneet arora, <puneetaroralnt@gmail.com> wrote:Dear All,--In Aramco project can we use API 5L Gr. B PSL-1 Pipe for PQR purpose only.With Regards,Puneet
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment