Re: [MW:29027] Mechanical test for Welder qualification

Hi, 

Can we accept the welders as per RT qualification?. If mechanical test omitted will be it violation of B31.8?.

Reg,
Ibrahim


On Sat, Feb 2, 2019, 10:17 AM Ramin Kondori <raminkondori@gmail.com wrote:
Because it is a repeated work, pipeline standards ask for DT and it is a right thing to do.
It is highly recommended to follow this method of qualification.
RT is not as effective as DT for screening good welders in pipeline projects.

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Thu, Jan 31, 2019 at 6:04 AM Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Gents,

Is it mandatory mechanical test qualification for welders as per ASME B31.8 sour gas service requirement as per clause B823.2?.

Qualification by RT is acceptable ?.


Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone