Hello All
,
I would greatly appreciate if someone can advise me on procedure qualification using AWS 5.8- BCuP-3 filler alloy ( F# 103 listed in QB ) involving Cu-Cu base metal.
The filler alloy is equally suitable to use either with fusion welding process e.g GTAW or by Torch Brazing.
The intended application is Cu-Cu ( C11000) & base metal thickness range 1/16"- 1/4"
UTS all weld for filler metal : ~36Ksi Elongn: 8%
UTS of Cu base plate ( UNS : C11000) : 42KSI
Concern is even with wrap around Bend Test failure will be in the WELD. if PQR test per QW ?
Advise best welding procedure to qualify WPS or BPS ( QW or QB) & acceptance ? Any one has any experience?
Thanks
Amitabh