Re: [MW:27607] Use of SA240 TP 304 WPS to weld SA240 TP 316

Yes you can, but revise WPS to address 316 filler wire

On Fri 30 Mar, 2018 11:53 pm chiluka venkatramulu, <ramuluchiluka@gmail.com> wrote:
Dear All,
Pl clarify the below.
Can I Use SA240 TP 304 WPS to weld SA240 TP 316 material
   OR
Shall I need to prepare other WPS  based on the above PQR

With best wishes,
Venkat

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...